After the magnets are molded they are heated to 935°C (± 5°) and cool in a magnetic field of proper shape and intensity. They are then held at 1290°C (± 5°) for the required time and held for one hour at 627°C (± 5°) and four hours at 550°C (± 5°). The magnets leave the aging process magnetized and are de-magnetized so they can be finished or surface ground to the proper dimensions.

We get all our Alnico magnets un-magnetized for special magnetizing and calibration. We have several magnetizers and custom built calibrators needed for special pickups and applications. I like using a DC Electromagnet and often use a permanent magnet to magnetize various pickups. We use an adjustable pole piece for various rod and bar magnets made from soft iron.

Please check your items carefully and confirm they are correct for color, position, etc. We are not able to accommodate order changes or cancellations once you have completed the check out process.

My cart
Your cart is empty.

Looks like you haven't made a choice yet.